PA66 德國巴斯夫 C3U
性能項目 | 測試條件 | 測試方法 | 數值/描述 | 單位 | |
機械性能 | 拉伸強度(引張強度) | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | ||
斷裂伸長率 | ASTM D638/ISO 527 | 5/>50 | % | ||
拉伸模量 | ASTM D638/ISO 527 | 3600-1500 | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | 85 | % | ||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | 45 | % | ||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 3000/ | kg·cm/cm(J/M)ft·lb/in | ||
彎曲強度 | ASTM D790/ISO 178 | kg·cm/cm(J/M)ft·lb/in | |||
洛氏硬度 | ASTM D785 | ||||
IZOD 缺口沖擊強度 | 1/4" 23℃ | ASTM D256/ISO 179 | 4.5/11 | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | 3.5 | kg·cm/cm(J/M)ft·lb/in | ||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強度 | 23℃ (缺口) | ASTM D256/ISO 179 | 9/35(4) | kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無缺口) | ASTM D256/ISO 179 | 100/NB(-) | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.16 | ||
成型收縮率 | ASTM D955 | % | |||
熔融指數(流動系數) | 200℃/5kg | ASTM D1238/ISO 1133 | >100 | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
吸水率 23℃/24H | ASTM D570/ISO 62 | 8-9 | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | ℃(℉) | |
未退火 | ASTM D648/ISO 75 | 243 | ℃(℉) | ||
維卡軟化點 | ASTM D1525/ISO R306 | ℃(℉) | |||
熔點 | - | 243 | ℃(℉) | ||
燃燒性(率) | UL94 | ||||
線性膨脹系數 | ASTM D696/ISO 11359 | 0.33 | mm/mm.℃ | ||
電氣性能 | 介電常數 | 100HZ | ASTM D150/IEC 60250 | ||
1MHZ | ASTM D150/IEC 60250 | ||||
體積電阻率 | ASTM D257/IEC 60093 | 1015/1011 | Ω.cm | ||
表面電阻率 | ASTM D257/IEC 60093 | 1012/1010 | Ω | ||
耐電弧性 | ASTM D495/IEC 60112 | ||||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||
熔體溫度 | ℃ | ||||
模具溫度 | ℃ | ||||
壓力 | 注塑壓力 | Mpa | |||
保壓壓力 | Mpa | ||||
背壓 | Mpa | ||||
螺桿轉速 | rpm |